Enhanced Guidelines for Grade 91 Steel

An updated technical report provides information on ordering, processing, and inspecting this material
May 2025
By: JOHN A. SIEFERT

Grade 91 steel was first codified in 1983 as Code Case 1943 for tubing. Additional code cases were adopted in 1986 for seamless pipe, forged pipe, forgings, and plate, followed by a code case in 1995 for castings. The widespread use of Grade 91 steel since the late 1990s coincided with the combined cycle boom in the United States and a worldwide supercritical coal-fired plant build-out that involved the installation of over 1000 miles of pipe and required hundreds of thousands of welds.

The worldwide supply c..

Join AWS to read the full article

Get access to key insights and premium industry news today!
Already a member? Log In

Search Articles 

Find past articles by date, topic, or keyword.

Publication Archive

View past issues of our magazines, including Welding Research Supplements in PDF format.

AWS News

Stay up to date on the latest announcements from AWS.