In-Space Laser Welding Technology Takes Flight

A NASA-OSU partnership conducts a welding experiment held in reduced-gravity conditions
April 2025
By: JEFFREY W. SOWARDS, ANDREW O’CONNOR, BOYD PANTON, AND ANTONIO J. RAMIREZ

Imagine a future where space is no longer a destination for a select few astronauts but a thriving industry hub where manufacturing beyond Earth’s atmosphere is routine. This is a future where factories orbit the planet, power stations generate life-giving energy for outposts on the surface of the Moon, and autonomous robots mine deep into asteroids to extract precious resources. Cutting-edge welding and manufacturing technologies will shape how structures are built, and a new workforce will emerge, bringing this f..

Join AWS to read the full article

Get access to key insights and premium industry news today!
Already a member? Log In

Search Articles 

Find past articles by date, topic, or keyword.

Publication Archive

View past issues of our magazines, including Welding Research Supplements in PDF format.

AWS News

Stay up to date on the latest announcements from AWS.