Making a WAAM System for Maritime Education and Research

Find out how students assembled this cost-effective equipment 
April 2023
By: JAMES GAROFALO, ANNIE BLADOW, AND KOLBE KIRLIN

The United States Merchant Marine Academy (USMMA) in New York, also known as Kings Point, is a federal service academy that educates and graduates licensed merchant marine officers and officers commissioning into the armed forces. The academy was started in 1943 and began producing merchant marine officers, which were in dire need at the time, to ship supplies overseas. Academy graduates abide by the motto “Acta Non Verba” or “Deeds Not Words” and often sail in the merchant shipping fleet, work in shipyards, or go ..

Join AWS to read the full article

Get access to key insights and premium industry news today!
Already a member? Log In

Search Articles 

Find past articles by date, topic, or keyword.

Publication Archive

View past issues of our magazines, including Welding Research Supplements in PDF format.

AWS News

Stay up to date on the latest announcements from AWS.